在冷拔复合管生产中,打头是必不可少的一道工序,目前生产厂家主要采用人工打头方式,使打头部分受力不均,复合管拉拔成型时容易造成内外两管贴合不紧密,直接影响其生产效率及产品质量。本文主要是针对冷把复合管打头的工艺要求,设计出满足其工艺要求的机械装置,装置适应管规格Φ20-Φ60,外管壁厚0.5mm,内管1.5mm,打头长度不大于200mm,打头一次成型。本装置传动系统采用齿轮传动,再通过凸轮机构将转动转换为平动,并带动模具打压复合管头,装置每分钟可打头6次,一次打头需时3秒,打头间隔时间3秒,成型后打头部分受力均匀,坚实紧密,成扁瓶状,从而节省人力并提高了生产效率及产品质量。
冷拔cold-drawn 复合管composite pipe 打头end-pointing 齿轮gear wheel 凸轮cam 模具anvil
在线等,急!第一次来,分都给你了,呵呵

In the composite drawing of the production, is essential to begin a process, the major manufacturers begin using artificial methods so that the beginning part of Shouli Bu all, the composite drawing of the molding easy for the two stickers inside and outside of not close, A direct impact on their production efficiency and product quality. This paper is mainly directed against the cold of the beginning of the process requirements, design technology to meet the requirements of the mechanical devices, devices meet the specifications Φ20-Φ60, pipe wall thickness of 0.5 mm, possession of 1.5 mm, beginning length of not more than 200 mm, Forming a first time. Transmission System using the device Gear, and then through the cam will rotate into translation and promote mold of suppressing the first, the installation of every six minutes beginning, a beginning to take three seconds, three seconds interval beginning, molding After the beginning of some of the uniform, a solid closer, a bottle-