换上φ35mm螺杆的注射机,打了50模后,产品表面没有黑纹,结合线上有细小黑纹。bayer的料制出来的产品上也有,证明这是生产技术上的问题,我们的材料质量上没问题。

方案:
明天制上下模,拿样品送OEM方检测看能不能pass.

Review: φ35 mm screw put on the injection machine, a 50-play, and no product surface profiling, with a small black online profile. bayer the material out of the products have to prove that this is the production of technical problems, we have the quality of the materials no problem. Programme: Die tomorrow system from top to bottom, with test samples sent to the OEM whether we can pass.

Review:

Φ35 mm screw put on the injection machine, a 50-play, and no product surface profiling, with a small black online profile. bayer the material out of the products have to prove that this is the production of technical problems, we have the quality of the materials no problem.